2025-12-28 22:58:10 UNS N05500蒙乃尔铜镍合金的制作工艺与泊松比
UNS N05500 经轧制,泊松比 0.3,含 Ni63% AlTi。执行 ASTM B164。...
了解详情
UNS N05500 经轧制,泊松比 0.3,含 Ni63% AlTi。执行 ASTM B164。...
了解详情
UNS N04405 室温抗拉≥550MPa,300℃≥500MPa,含 Ni65% Cu。执行 ASTM B164。...
了解详情
UNS N04400 冲击韧性≥20J/cm²,比热容 0.46J/g・℃,含 Ni65% Cu。执行 ASTM B164。...
了解详情
UNS N10276 零件经退火,抗拉≥690MPa,含 Ni15-17% Mo15-17%。执行 ASTM B622。...
了解详情
UNS N07750 组织奥氏体,易冲压,含 Ni70% Cr15% Co。执行 ASTM B637。...
了解详情